Parameter |
|
Typical Value |
Unit |
Method |
|
Density |
|
1.19 |
gr/cm3 |
ISO 2781 |
|
Shore Hardness |
|
91 |
A |
ISO 7619-1 |
|
Abrasion Loss |
|
30 |
mm3 |
ISO 4649 |
|
Tensile Modulus: |
50% 100% 300% |
7.4 9.5 28.2 |
N/mm2 |
ISO 22654 |
|
Tensile Strength |
|
63.5 |
N/mm2 |
ISO 22654 |
|
Elongation at Break |
|
450 |
% |
ISO 22654 |
|
Tear Strength |
|
105 |
N/mm |
ISO 34-1 |
|
Vicat Softening Point |
|
125 |
°C |
ISO 306 |
|
Compression set: |
70h/23°C 22h/70°C |
22 40 |
% |
ISO 815-1 |
|
Zone |
Temperature |
|
Zone 1 |
190°C |
|
Zone 2 |
195°C |
|
Zone 3 |
200°C |
|
Nozzle |
195°C |
|
Zone |
Temperature |
|
Zone 1 |
190°C |
|
Zone 2 |
195°C |
|
Zone 3 |
200°C |
|
Zone 4 |
195°C |
|
Adapter |
190°C |
|
Die |
185°C |